Weber Saint-Gobain - Official website of the company

weber.color poxy

weber.color poxy
weber.color poxy

Product Benefits

  • Excellent chemical and high acidity resistant property
  • Resist to temperature from -40°C to +100°C
  • For joint width from 2 to 12 mm without crack 
  • Anti-bacteria and anti-infection properties

Excellent-performance epoxy tile adhesive and grout with maximum long-lasting property

Product Features

Key Benefits

  • Resist to chemical and high acidity
  • Anti-bacteria and anti-infection properties
  • Ideal for use with the areas where heavy-duty property is required
  • Resist to temperature from -40°C to +100°C (+180°C in case of thermal shock)
  • Resist to water pressure in swimming pools
  • Available in 4 colors
  • For joint width 2-12 mm without crack

Technical Data

  • Pot life (in shade) : 30 minutes
  • Hardening time : 4 - 8 hours
  • Optimum time for chemical resistance
    • 4 days at 20oC or
    • 8 days at 10oC
  • Temperature resistance : -40oC to + 100oC Up to + 180oC in caseof thermal shock
  • Bonding strength in dry condition : > 3 N/mm2
  • Bonding strength in wet condition : > 3 N/mm2
  • pH : 10 - 11
    • Remark: These test results are from laboratory test. They could be slightly different from on-site results because of the differences in applications and conditions.

ข้อจำกัดในการใช้งาน

ตารางคุณสมบัติทนทานต่อสารเคมีของ เวเบอร์.คัลเลอร์ พ๊อกซี่

Certified Standard

Epoxy Adhesive

International/European standard

  • Standard Result Initial shear adhesion strength ISO 13007 part 2-4.3.4 or EN 12003-7.2
    • Standard ≥ 2 N/mm2 l Result 8.4 N/mm2
  • Shear adhesion strength after water immersion ISO 13007 part 2-4.3.5 or EN 12003-7.3
    • Standard ≥ 2 N/mm2 l Result 7.4 N/mm2
  • Shear adhesion strength after thermal shock ISO 13007 part 2-4.3.8 or EN 12003-7.5
    • Standard ≥ 2 N/mm2 l Result 9.9 N/mm2
  • Open time tensile adhesion strength ISO13007 part 2-4.1 or EN 1346
    • Standard ≥ 0.5 N/mm2 l Result 4.2 N/mm2

Epoxy Grout

International/European standard

  • Abrasion resistance ISO 13007 part 4-4.4 or EN 12808-2
    • Standard ≤ 250 mm3 l Result 67 mm3
  • Flexural strength under standard condition ISO 13007 part 4-4.1.3 or EN 12808-3
    • Standard ≥ 30 N/mm2 l Result 30 N/mm2
  • Compressive strength under standard condition ISO 13007 part 4-4.1.4 or EN 12808-3
    • Standard ≥ 45 N/mm2 l Result 64.38 N/mm2
  • Shrinkage ISO 13007 part 4-4.3 or EN 12808-4
    • Standard ≤ 1.5 mm./m l Result 0.46 mm./m
  • Water absorption after 240 minutes ISO 13007 part 4-4.2 or EN 12808-5
    • Standard ≤ 0.1 g l Result 0.00 g

 

 

Documentation

Send or download the documentation

You can either send the documentation to en-email address, or download it.

Application

Substrate preparation

  • The joints should be clean and dry before grouting. 
  • Clean and remove any particles or contaminations remaining in the joints in order to ensure a good grout adhesion and the color uniformity.  

Mixing

  • Mix the 2 components together by the ratio of 1:3 (upper part: lower part).  Stir the mixture until homogenious paste is obtained.
    • After proper mix, leave the product for 3 to 4 minutes before using in order to have the complete chemical reaction. 
  • The mixture of weber.color poxy should be used within 30 minutes and kept away from heat & sunlight.  

 

 

Application

  • For wall: Use weber rubber trowel or an appropriate tool to fill tile joints diagonally.    
  • For floor: Apply the mixed grout onto the area of 1 m2, and then use the rubber trowel to diagonally fill the joints.
  • After 15 to 20 minutes or after filling the joint on the area of 1 m2, wipe off any excess grout from tile surfaces with warm-damp abrasive sponge
  • Clean off the excess grout again with warm-damp sponge to ensure there is no excess of weber.color poxy left on the surfaces.
  • Wait for 4 - 8 hours to ensure the good bonding of grout.
    • The optimum hardening time and the optimum time to resist chemical is 4 days at 20°C or 8 days at 10°C  

Application property

  • Pot life: 30 minutes
  • Hardening time: 4 to 8 hours
  • Optimum hardening and chemical-resistant time:
    • 4 days at 20°C and
    • 8 days at 10°C
  • Time before traffic: 4 to 8 days  

Packaging

Packaging

  • 5 kg bucket (One bucket can use with the area of 8 m2 approximately)  

Shelf Life & Storage

  • One year after manufacturing date when stored unopened in dry and ventilated place (store airtight in dry and ventilated conditions, if remained in opened bag)